Line 3 — Injection moulding
Mould clamp pressure drifting after 90 minutes of running; short shots on cavity 3.
Action
Hydraulic team to check accumulator pre-charge before C shift.
Shift log · 27 Nov 2026
Output, rejections, downtime, every checksheet reading against its spec window, and what the operators actually saw on the floor — one entry screen for all three.
Produced today
1,571
plan 1,600 · 98% attainment
Rejection rate
1.87%
30 pcs rejected
Downtime logged
77 min
across all shifts
Checks out of spec
2/5
parameter readings today
Open observations
2
1 high severity
01 · Daily production data
One row per line, per shift. Attainment and rejection percentage are calculated the moment you save.
Line 4 — Assembly
27 Nov · B · 14:00–22:00
CV-90 cover plate · A. Qureshi
Line 3 — Injection moulding
27 Nov · A · 06:00–14:00
HX-311 housing · S. Fernandes
Line 2 — CNC cell
27 Nov · A · 06:00–14:00
SL-18 shaft · R. Kulkarni
Line 1 — Press shop
26 Nov · C · 22:00–06:00
HX-204 bracket · M. Bhosale
| Date | Shift | Line | Part | Plan | Produced | Rej. | Rej. % | DT | Operator | Actions |
|---|---|---|---|---|---|---|---|---|---|---|
| 27 Nov | B · 14:00–22:00 | Line 4 — Assembly | CV-90 cover plate | 520 | 538 103% | 4 | 0.7% | 12m | A. Qureshi | |
| 27 Nov | A · 06:00–14:00 | Line 3 — Injection moulding | HX-311 housing | 600 | 571 95% | 19 | 3.2% | 41m | S. Fernandes | |
| 27 Nov | A · 06:00–14:00 | Line 2 — CNC cell | SL-18 shaft | 480 | 462 96% | 7 | 1.5% | 24m | R. Kulkarni | |
| 26 Nov | C · 22:00–06:00 | Line 1 — Press shop | HX-204 bracket | 450 | 404 90% | 22 | 5.2% | 65m | M. Bhosale |
02 · Checksheet parameters
Enter the spec window once per parameter and the reading is judged in spec, below or above — no mental arithmetic on the floor.
Coating thickness
27 Nov · B · 14:00–22:00
Line 5 — Paint & cure · P. Deshmukh
Cycle time
27 Nov · B · 14:00–22:00
Line 3 — Injection moulding · N. Iyer
Barrel temperature
27 Nov · A · 06:00–14:00
Line 3 — Injection moulding · N. Iyer
Bore diameter
27 Nov · A · 06:00–14:00
Line 2 — CNC cell · D. Pawar
Shaft OD
27 Nov · A · 06:00–14:00
Line 2 — CNC cell · D. Pawar
| Date | Line | Parameter | Spec | Reading | Result | Inspector | Actions |
|---|---|---|---|---|---|---|---|
| 27 Nov | Line 5 — Paint & cure | Coating thickness B · 14:00–22:00 | 60 – 90 µm | 57.5 µm | Below spec | P. Deshmukh | |
| 27 Nov | Line 3 — Injection moulding | Cycle time B · 14:00–22:00 | 38 – 44 sec | 41.6 sec | In spec | N. Iyer | |
| 27 Nov | Line 3 — Injection moulding | Barrel temperature A · 06:00–14:00 | 215 – 235 °C | 228 °C | In spec | N. Iyer | |
| 27 Nov | Line 2 — CNC cell | Bore diameter A · 06:00–14:00 | 11.95 – 12.05 mm | 12.09 mm | Above spec | D. Pawar | |
| 27 Nov | Line 2 — CNC cell | Shaft OD A · 06:00–14:00 | 24.9 – 25.1 mm | 25.02 mm | In spec | D. Pawar |
03 · Observations
Machine behaviour, material issues, near misses. Each one carries a severity, an owner and an action until it is closed.
Mould clamp pressure drifting after 90 minutes of running; short shots on cavity 3.
Action
Hydraulic team to check accumulator pre-charge before C shift.
Coating thickness trending below 60 µm on the left-hand gun.
Action
Nozzle cleaned, re-check 5 panels every hour.
Coolant spill near press 2 walkway, housekeeping informed.
Action
Absorbent mat placed, floor marking repainted.
Production, quality and maintenance read the same log at the 7 a.m. meeting — today's attainment is 98% with 2 open observations.